One of the primary performance attributes of a high-performance weather-resistant barrier (WRB) is its ability to stand up to UV exposure. This is a critical point of differentiation between weather barriers, as prolonged exposure to UV radiation can cause material degradation, leading to loss of tensile strength, delamination of surface layers and reduced water repellency of the WRB. This is especially true in commercial construction where there are already prolonged construction schedules that are often slowed by a number of factors. For these reasons, it’s critical that UV exposure is top of mind when selecting a system of weather protection products. The Science of UV ExposureThe sun’s UV energy reaches the earth in a wide range of wavelengths, most of which are invisible. This UV radiation is commonly divided into three groups: UV A, B, and C rays.

  • UV-A (315 - 400) - closest to visible light
  • UV-B (280 – 315 nm) 
  • UV-C (less than 280 nm)

For context, UV-A wavelengths are what causes your skin to burn while UV-B are able to more deeply penetrate chromosomes of living cells causing more damage. UV-C are the shortest wavelengths and those most absorbed by the earth’s ozone. UV rays are measured in nanometers– or 1 billionth of a meter. The shorter the wavelength, the higher the energy level increasing its ability to damage exposed materials. Within the three groups of UV rays, the combination of UV-A and UV-B wavelengths are what impact the durability of many building materials. Long-term exposure can cause discoloration, loss of tensile strength, delamination of surface layers and reduced water repellency. Manufacturers assign housewrap a UV-rating based on characteristics like strength and water resistance after the product has had UV exposure. The rating then allows users to know the maximum time the wrap can withstand sun exposure without its performance degrading. Many housewraps currently on the market only offer up to 120 days of UV resistance. The TYPAR Weather Protection System—including TYPAR BuildingWrap, Flashing and Tape—offers up to six months of UV resistance without degradation to its performance capabilities, outperforming competing housewraps. While the goal should be to clad the exterior of the building as quickly as possible, projects are often delayed, leaving WRB’s vulnerable to longer than expected exposure to the sun. In these instances, WRBs like TYPAR MetroWrap™ are ideal due to the material’s ability to stand up to sunlight. It can be left exposed for up to 12 months with no UV degradation – more than any other product on the market. To learn more about the TYPAR Weather Protection System, visit www.typar.com.

×